73
Grammage m² | 420g/m² +/-5% |
Composition | 100% rPES |
Usable width | min. 140cm |
Martindale Test | 90 000->100 000 |
Thread displacement | 0,5-0,7 mm WARP / 1,1-1,3 mm WEFT |
Skłonność do mechacenia i pillingu | 3-4 |
Fastness to rubbing dry | light-5 / medium-4-5 / dark-4-5 |
Fastness to rubbing wet | light-4-5 / medium-5 / dark-4-5 |