54
Grammage m² | 380g/m² +/-5% |
Composition | 100% Polyester |
Usable width | min. 140cm |
Martindale Test | 80000-90000 |
Thread displacement | 2,1-2,5 mm WARP / 1,4-1,6 mm WEFT |
Skłonność do mechacenia i pillingu | 4-5 |
Fastness to rubbing dry | light-4-5 / medium-4-5 / dark-4-5 |
Fastness to rubbing wet | light-4-5 / medium-4-5 / dark-4-5 |