70
| Grammage m² | 380g/m² +/-10% |
| Composition | 92%PES 8%NY |
| Usable width | min. 140cm |
| Martindale Test | 90 000-100 000 |
| Thread displacement | 2,1-2,4 mm WARP / 2,3-2,5 mm WEFT |
| Skłonność do mechacenia i pillingu | 4 |
| Fastness to rubbing dry | light-5 / medium-5 / dark-4 |
| Fastness to rubbing wet | light-5 / medium-4-5 / dark-4-5 |