75
Grammage m2 | 340g/m² +/-5% |
Composition | 95%PES 5%NY |
Usable width | min. 140cm |
Martindale Test | 45000- 60000 |
Thread displacement | 2,6-3,0 mm WARP / 2,1-2,5 mm WEFT |
Skłonność do mechacenia i pillingu | 4 |
Fastness to rubbing dry | light-5 / medium-4-5 / dark-4-5 |
Fastness to rubbing wet | light-5 / medium-4-5 / dark-4-5 |