05
| Grammage m² | 230g/m² +/-5% |
| Composition | 100% Polyester |
| Usable width45000-50000 | min. 140cm |
| Martindale Test | 30000-40000 |
| Thread displacement | 2,8-3,2 mm WARP / 2,9-3,3 mm WEFT |
| Skłonność do mechacenia i pillingu | 4-5 |
| Fastness to rubbing dry | 4-5 |
| Fastness to rubbing wet | 4 |