88
| Grammage m² | 325g/m² +/-10% |
| Composition | 100% Polyester |
| Usable width | min. 140cm |
| Martindale Test | >100000 |
| Thread displacement | 3,4-3,8 mm WARP / 2,7-3,3 mm WEFT |
| Skłonność do mechacenia i pillingu | 4-5 |
| Fastness to rubbing dry | 5 |
| Fastness to rubbing wet | 5 |
| Grammage m² | 325g/m² +/-10% |
| Composition | 100% Polyester |
| Usable width | min. 140cm |
| Martindale Test | >100000 |
| Thread displacement | 3,4-3,8 mm WARP / 2,7-3,3 mm WEFT |
| Skłonność do mechacenia i pillingu | 4-5 |
| Fastness to rubbing dry | 5 |
| Fastness to rubbing wet | 5 |