99

Grammage m² 600g/m² +/-5%
Composition 70% rPES 30% PES
Usable width min. 140cm
Martindale Test 60000-70000
Thread displacement 1,9-2,1 mm WARP / 2,6-2,8 mm WEFT
Skłonność do mechacenia i pillingu 4
Fastness to rubbing dry light-5 / medium-4 / dark-4
Fastness to rubbing wet light-5 / medium-4-5 / dark-4-5