77
Grammage m² | 340g/m² +/-5% |
Composition | 88%PES 9%RA 3%NY |
Usable width | min. 140cm |
Martindale Test | 60000-70000 |
Thread displacement | 1,5-1,7 mm WARP / 1,2-1,4 mm WEFT |
Skłonność do mechacenia i pillingu | 4 |
Fastness to rubbing dry | light-5 / medium-4-5 / dark-4-5 |
Fastness to rubbing wet | light-5 / medium-5 / dark-4-5 |